Mill Roll
Roughing
- 1. Adamite (ADM)
High Carbon series Mill Roll, Impact Resistance (Toughness),Wear Resistance, Thermal Crack Resistance
Hardness : HS40~60
Micrograph :
420N (Hs 55/60) X 50
420N (Hs 55/60) X 100
Property : Excellent Toughness, Applying for Heavy Load Condition
- 2. Ductile Cast Iron (DCI)
Spherodal graphite Mill Roll, Impact Resistance (Toughness), Wear Resistance, Thermal Crack Resistance
Hardness : HS35~70
Micrograph :
160S (Hs 55/60) X 100
155H (Hs 45/50) X 100
Property : Exellent surface quality, relatively High Toughness, Wide Application
Intermediate
- 1. Ductile Cast Iron (DCI)
- 2. High Speed Steel (HSS)
MC Carbide and Martensite formation – Hot Hardness, High Toughness
Hardness : HS70~85
Micrograph :
270D (Hs 67/70) X 50
270D(Hs 67/70) X 100
Property : Excellent Wear Resistance, Excellent Surface quality(Cooling Condition Required)
- 3. Powder Metallurgy Alloy (FT-9)
Sintered Powder Product (HIP), Fine Carbide
– Excellent Wear ResistanceHardness : HS62~69
Micrograph :
Property : Excellent Wear Resistance, Excellent Surface Quality, Fulfilling Cost-down by Extending Roll Life Time
Finishing
- 1. Ductile Cast Iron (DCI)
- 2. High Speed Steel (HSS)
- 3. Powder Metallurgy Alloy (FT-9)
- 4. Tungsten Carbide (WC)
Powder Metallurgy Product, Excellent Wear Resistance
Hardness : HS71~99
Micrograph :
Property : Excellent Wear Resistance & Surface Quality, Easy to crack by Rapid Temperature Change & Impact